All I can say is wow. This sale was insane. Turnout was much larger than we expected but I do believe that we got everyone taken care of. And a huge thanks goes out to Max for keeping everything rolling smooth on Faebook. Thank you to all who stayed up with us to get in on these deals. And be proud of yourself for supporting an American owned and operated small business, we really appreciate!
-
This test represents a "best case scenario" by having the sheet metal perfect flat. The results would be pretty similar to that in a car environment. If someone would be willing to pay for a car door or a test vehicle for me to do these tests, then I'd be more than happy to do yet another run. Also this testing method is similar to the standard Oberst Bar (SAE J1637, ASTM E-756) test which is used to test these products, just a poor man's version. Yes that is correct, P&S could come close to the results of a CLD, but isn't the point of using P&S over a properly designed CLD to save money? With the prices you provided, you were able to buy the P&S at 40¢-41¢ a sq. ft.. With two layers (to achieve similar results of that of just 25% coverage with a CLD), you paid 8 0¢-.82¢ per square foot of coverage. With the CLD I used, which on the high side is around $3.50 a sq. ft., since only a quarter of that needs to be used, that is 87¢-88¢ to treat the same area. So at BEST you are saving 6¢ a sq. ft. by using P&S over the CLD. If you have 100 sq. ft. of surface area to treat, by using P&S you can save a total of $6 over using a CLD. Personally, my time is worth more than $6. I'm not flat out saying that P&S won't work... hell using multiple layers of duct tape would do something. What I'm saying that it's not worth the time, effort, or even the money to use P&S as sound deadener. It's not cheaper to achieve similar results. It can smell (not all do). Can be unhealthy (again not all) if installed in a closed/sealed environment such as a car. It weighs more. Takes more time to install. A pain in the ass to cleanup. Has a high failure rate vs. CLDs. Etc., etc.
-
Oh yeah there are many ways I can test these placement theories and see if there is any difference between them. Might just have to waste more product and do another round. On a door panel where you have areas that are welded or reinforced, those areas would obviously dictate that no product would need to be used there. So staying away from the edges (were the panel would not resonate or vibrate as much or at all) would be much more beneficial. I'll hug yer nuts! Glad I was able to convince you to some degree. But in all seriousness all I am trying to show is that these sort of materials do not nor will not work as well as a constrained layer damper. So if anything just use one of the many high quality CLDs that are out there. Dynamat, Stinger RoadKill, SDS CLD Tiles, and our products (obviously) are my favorites based on how well they perform and I personally would not hesitate to use any of them.
-
I'm a bit tired, so I'll make this short and answer the questions a bit more in depth in the morning. But yeah the last two examples are a bit extreme (the pieces are far too small to act as a constraining system), thus it would not be an effective way to treat the panel. In theory, pretty much any arrangement achieving the same surface area would work so long as the CLD is large enough, but again that is in theory.
-
I don't think it really matters as to where you apply it on the surface, but rather the amount of coverage. For instance this is how most have been (myself included) installing it for a while now, as close to the middle as you can. But you could also use the same amount of product and space it out like this: And you would be treating the same surface area. Or you could go nuts and do something like this: Or even this: Again, you are using the same amount of product, just applying it all over the panel.
-
Ok, went out and did the 100% CLD test as request. The fun part was removing the two layers of the U-Seal. I'll give credit to this product for being sticky as hell in 75° temps. So I got it all cleaned off and applied 1 sq. ft. of the CLD product onto the testing area. I had to be creative and cut up multiple sheets to make sure there wasn't any logos, printed things, or any tell-tale signs as to what product I am using. Three runs, taking the average, and here are the results. The 100% CLD applied over the 100% U-Seal U-Seal = BLUE CLD = GREEN Now the 100% U-Seal applied over the 100% CLD U-Seal = RED CLD = BLUE Now 100% U-Seal with 25% CLD and 100% CLD: The interesting part that I noticed is that at around the 27 second mark the U-Seal does better. Here is a zoomed in section from about 26.70 seconds to 30.40 seconds. Interesting hu? So there you go more data to chew on. Final conclusion Sure with 100% coverage you do achieve even better results. However in some cases it's not that much, if any, better than 25% coverage.