Ricky A. Posted December 22, 2010 Report Posted December 22, 2010 how long should i wait between layers when im making my box? i wanna do this right lol thanks yall BUILD LINK: http://www.stevemeadedesigns.com/board/topic/112034-2-sundown-18s-98-f-150/page__p__1565972__fromsearch__1#entry156597298 Ford F-150Truck:37" superswamper tsl radials16" ion alloy wheels3" body lift2" suspension liftOffbrand brushguardPIAA driving lights6000K HID'sSystem:2 18" Sundown NightshaedAq3500Custom Fiberglass boxfosgate T1 6x8 Coxialsbass inferno 2000 watt 4 channel2 XS power d3100's0 Gauge
finkster Posted December 22, 2010 Report Posted December 22, 2010 It all depends on how much hardener you used and what the temperature is. Make sure its completely cured before adding another layer. DAT 4125------>RE XXX comps active Eclipse cd7000 I serve drunks for a living
Ricky A. Posted December 22, 2010 Author Report Posted December 22, 2010 oh ok thanks that was my main question. so i do need to let it cure first. btw im doing 3 to 1 resin to hardner and its like 45 to 55 her in bama BUILD LINK: http://www.stevemeadedesigns.com/board/topic/112034-2-sundown-18s-98-f-150/page__p__1565972__fromsearch__1#entry156597298 Ford F-150Truck:37" superswamper tsl radials16" ion alloy wheels3" body lift2" suspension liftOffbrand brushguardPIAA driving lights6000K HID'sSystem:2 18" Sundown NightshaedAq3500Custom Fiberglass boxfosgate T1 6x8 Coxialsbass inferno 2000 watt 4 channel2 XS power d3100's0 Gauge
Sanitarium Posted December 22, 2010 Report Posted December 22, 2010 3 to 1? Shits ginna start smokin... You can do 3 layers of cloth as long as you're not uaing too much resin. You want just enough to get the cloth wet.
Superjay Posted December 22, 2010 Report Posted December 22, 2010 don't wait at ALL!!!! if you wait, wait 4-5 hours with a sanding between them. Principal JTech Consulting - Leader in 12-Volt Training and Product PlanningIt's not about how much power you have, but how well you use it
mbdblue Posted December 22, 2010 Report Posted December 22, 2010 don't wait at ALL!!!! if you wait, wait 4-5 hours with a sanding between them. ^this. and if its only 45-55 degrees out, your gonna wanna hit it with a heat gun or be prepared to leave it for a while after your done. the lower the temp is, the longer its gonna take to cure. AA-Atomic-Clif Designs-DC-Diamond-Digital Designs-Directed-Eclipse-Fi-Hertz-Hifonics-Kenwood-Memphis-Phoenix Gold-Pioneer-PPI-PSi-Stinger-Sundown-TC Sounds-Viper-Zapco
Superjay Posted December 22, 2010 Report Posted December 22, 2010 or put more MEKP into it. I always cook hot anyway, but if it's raining, or cold out you're going to need MORE (sometimes double) the catalyst to amke it cure correctly. It shouldn't get so hot you can't touch it...that leads to cracking Principal JTech Consulting - Leader in 12-Volt Training and Product PlanningIt's not about how much power you have, but how well you use it
Recommended Posts
Archived